High-Temperature low cycle fatique properties of oxide despersion strengthened superalloy MA 6000. / Hynnä, A.; Kuokkala, V.-T.; Mäntylä, T.; Kettunen, P.

Tampere : Tampere University of Technology, 1985. 21 p. (Tampere University of Technology, Institute of Materials Science, Report; No. 37/1985).

Research output: Book/ReportCommissioned reportProfessional

Harvard

Hynnä, A, Kuokkala, V-T, Mäntylä, T & Kettunen, P 1985, High-Temperature low cycle fatique properties of oxide despersion strengthened superalloy MA 6000. Tampere University of Technology, Institute of Materials Science, Report, no. 37/1985, Tampere University of Technology, Tampere.

APA

Hynnä, A., Kuokkala, V-T., Mäntylä, T., & Kettunen, P. (1985). High-Temperature low cycle fatique properties of oxide despersion strengthened superalloy MA 6000. (Tampere University of Technology, Institute of Materials Science, Report; No. 37/1985). Tampere: Tampere University of Technology.

Vancouver

Hynnä A, Kuokkala V-T, Mäntylä T, Kettunen P. High-Temperature low cycle fatique properties of oxide despersion strengthened superalloy MA 6000. Tampere: Tampere University of Technology, 1985. 21 p. (Tampere University of Technology, Institute of Materials Science, Report; 37/1985).

Author

Hynnä, A. ; Kuokkala, V.-T. ; Mäntylä, T. ; Kettunen, P. / High-Temperature low cycle fatique properties of oxide despersion strengthened superalloy MA 6000. Tampere : Tampere University of Technology, 1985. 21 p. (Tampere University of Technology, Institute of Materials Science, Report; 37/1985).

Bibtex - Download

@book{9c33652c0388491088bbc991a0702a27,
title = "High-Temperature low cycle fatique properties of oxide despersion strengthened superalloy MA 6000",
author = "A. Hynn{\"a} and V.-T. Kuokkala and T. M{\"a}ntyl{\"a} and P. Kettunen",
note = "Contribution: organisation=mol,FACT1=1",
year = "1985",
language = "English",
series = "Tampere University of Technology, Institute of Materials Science, Report",
publisher = "Tampere University of Technology",
number = "37/1985",

}

RIS (suitable for import to EndNote) - Download

TY - BOOK

T1 - High-Temperature low cycle fatique properties of oxide despersion strengthened superalloy MA 6000

AU - Hynnä, A.

AU - Kuokkala, V.-T.

AU - Mäntylä, T.

AU - Kettunen, P.

N1 - Contribution: organisation=mol,FACT1=1

PY - 1985

Y1 - 1985

M3 - Commissioned report

T3 - Tampere University of Technology, Institute of Materials Science, Report

BT - High-Temperature low cycle fatique properties of oxide despersion strengthened superalloy MA 6000

PB - Tampere University of Technology

CY - Tampere

ER -