Roll-to-roll atomic layer deposition for flexible substrates
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution › Scientific › peer-review
Details
Original language | English |
---|---|
Title of host publication | TAPPI International Conference on Nanotechnology 2013 |
Publisher | TAPPI Press |
Pages | 726-739 |
Number of pages | 14 |
ISBN (Electronic) | 9781510815681 |
Publication status | Published - 2013 |
Publication type | A4 Article in a conference publication |
Event | TAPPI International Conference on Nanotechnology 2013 - Stockholm, Sweden Duration: 24 Jun 2013 → 27 Jun 2013 |