1.4 µm continuous-wave diamond Raman laser

Tutkimustuotosvertaisarvioitu

Yksityiskohdat

AlkuperäiskieliEnglanti
Sivut31377-31383
Sivumäärä7
JulkaisuOptics Express
Vuosikerta25
Numero25
DOI - pysyväislinkit
TilaJulkaistu - 11 joulukuuta 2017
OKM-julkaisutyyppiA1 Alkuperäisartikkeli

Tiivistelmä

The longest wavelength (~1.4 µm) emitted by a diamond Raman laser pumped by a semiconductor disk laser (SDL) is reported. The output power of the intracavity-pumped Raman laser reached a maximum of 2.3 W with an optical conversion efficiency of 3.4% with respect to the absorbed diode pump power. Narrow Stokes emission (FWHM <0.1 nm) was attained using etalons to limit the fundamental spectrum to a single etalon peak. Tuning of the Raman laser over >40 nm was achieved via rotation of an intracavity birefringent filter that tuned the SDL oscillation wavelength.