A novel thermotropic elastomer based on highly-filled LDH-SSB composites

Tutkimustuotosvertaisarvioitu

Standard

A novel thermotropic elastomer based on highly-filled LDH-SSB composites. / Das, Amit; George, Jinu Jacob; Kutlu, Burak; Leuteritz, Andreas; Wang, De Yi; Rooj, Sandip; Jurk, René; Rajeshbabu, Ramanujam; Stöckelhuber, Klaus Werner; Galiatsatos, Vassilios; Heinrich, Gert.

julkaisussa: Macromolecular Rapid Communications, Vuosikerta 33, Nro 4, 27.02.2012, s. 337-342.

Tutkimustuotosvertaisarvioitu

Harvard

Das, A, George, JJ, Kutlu, B, Leuteritz, A, Wang, DY, Rooj, S, Jurk, R, Rajeshbabu, R, Stöckelhuber, KW, Galiatsatos, V & Heinrich, G 2012, 'A novel thermotropic elastomer based on highly-filled LDH-SSB composites', Macromolecular Rapid Communications, Vuosikerta. 33, Nro 4, Sivut 337-342. https://doi.org/10.1002/marc.201100735

APA

Das, A., George, J. J., Kutlu, B., Leuteritz, A., Wang, D. Y., Rooj, S., ... Heinrich, G. (2012). A novel thermotropic elastomer based on highly-filled LDH-SSB composites. Macromolecular Rapid Communications, 33(4), 337-342. https://doi.org/10.1002/marc.201100735

Vancouver

Das A, George JJ, Kutlu B, Leuteritz A, Wang DY, Rooj S et al. A novel thermotropic elastomer based on highly-filled LDH-SSB composites. Macromolecular Rapid Communications. 2012 helmi 27;33(4):337-342. https://doi.org/10.1002/marc.201100735

Author

Das, Amit ; George, Jinu Jacob ; Kutlu, Burak ; Leuteritz, Andreas ; Wang, De Yi ; Rooj, Sandip ; Jurk, René ; Rajeshbabu, Ramanujam ; Stöckelhuber, Klaus Werner ; Galiatsatos, Vassilios ; Heinrich, Gert. / A novel thermotropic elastomer based on highly-filled LDH-SSB composites. Julkaisussa: Macromolecular Rapid Communications. 2012 ; Vuosikerta 33, Nro 4. Sivut 337-342.

Bibtex - Lataa

@article{f1240ba9778148059475cbbf8ccb01dc,
title = "A novel thermotropic elastomer based on highly-filled LDH-SSB composites",
abstract = "Elastomeric composites are prepared based on solution styrene butadiene elastomer and zinc-aluminium layered double hydroxides (LDH), using a conventional sulphur cure system. Up to 100 parts per hundred rubber of LDH are incorporated into the elastomer matrix. The composites exhibit an interesting phenomenon of thermoreversible transparency, i.e. the transparent sample becomes opaque at warm condition and restores the transparency at room temperature. The transparency is found to be increased as the amount of LDH was increased. The addition of LDH gradually improved the mechanical, dynamic mechanical performance and thermal stability of the base elastomer. These developped elastomers could be utilised as smart materials in different applications",
author = "Amit Das and George, {Jinu Jacob} and Burak Kutlu and Andreas Leuteritz and Wang, {De Yi} and Sandip Rooj and Ren{\'e} Jurk and Ramanujam Rajeshbabu and St{\"o}ckelhuber, {Klaus Werner} and Vassilios Galiatsatos and Gert Heinrich",
year = "2012",
month = "2",
day = "27",
doi = "10.1002/marc.201100735",
language = "English",
volume = "33",
pages = "337--342",
journal = "Macromolecular Rapid Communications",
issn = "1022-1336",
publisher = "Wiley-VCH Verlag",
number = "4",

}

RIS (suitable for import to EndNote) - Lataa

TY - JOUR

T1 - A novel thermotropic elastomer based on highly-filled LDH-SSB composites

AU - Das, Amit

AU - George, Jinu Jacob

AU - Kutlu, Burak

AU - Leuteritz, Andreas

AU - Wang, De Yi

AU - Rooj, Sandip

AU - Jurk, René

AU - Rajeshbabu, Ramanujam

AU - Stöckelhuber, Klaus Werner

AU - Galiatsatos, Vassilios

AU - Heinrich, Gert

PY - 2012/2/27

Y1 - 2012/2/27

N2 - Elastomeric composites are prepared based on solution styrene butadiene elastomer and zinc-aluminium layered double hydroxides (LDH), using a conventional sulphur cure system. Up to 100 parts per hundred rubber of LDH are incorporated into the elastomer matrix. The composites exhibit an interesting phenomenon of thermoreversible transparency, i.e. the transparent sample becomes opaque at warm condition and restores the transparency at room temperature. The transparency is found to be increased as the amount of LDH was increased. The addition of LDH gradually improved the mechanical, dynamic mechanical performance and thermal stability of the base elastomer. These developped elastomers could be utilised as smart materials in different applications

AB - Elastomeric composites are prepared based on solution styrene butadiene elastomer and zinc-aluminium layered double hydroxides (LDH), using a conventional sulphur cure system. Up to 100 parts per hundred rubber of LDH are incorporated into the elastomer matrix. The composites exhibit an interesting phenomenon of thermoreversible transparency, i.e. the transparent sample becomes opaque at warm condition and restores the transparency at room temperature. The transparency is found to be increased as the amount of LDH was increased. The addition of LDH gradually improved the mechanical, dynamic mechanical performance and thermal stability of the base elastomer. These developped elastomers could be utilised as smart materials in different applications

UR - http://www.scopus.com/inward/record.url?scp=84863149624&partnerID=8YFLogxK

U2 - 10.1002/marc.201100735

DO - 10.1002/marc.201100735

M3 - Article

VL - 33

SP - 337

EP - 342

JO - Macromolecular Rapid Communications

JF - Macromolecular Rapid Communications

SN - 1022-1336

IS - 4

ER -