Atomic layer deposition on polymer based flexible packaging materials: Growth characteristics and diffusion barrier properties

Tutkimustuotosvertaisarvioitu

Standard

Atomic layer deposition on polymer based flexible packaging materials: Growth characteristics and diffusion barrier properties. / Kääriäinen, Tommi O.; Maydannik, Philipp; Cameron, David C.; Lahtinen, Kimmo; Johansson, Petri; Kuusipalo, Jurkka.

julkaisussa: Thin Solid Films, Vuosikerta 519, Nro 10, 2011, s. 3146-3154.

Tutkimustuotosvertaisarvioitu

Harvard

APA

Vancouver

Author

Kääriäinen, Tommi O. ; Maydannik, Philipp ; Cameron, David C. ; Lahtinen, Kimmo ; Johansson, Petri ; Kuusipalo, Jurkka. / Atomic layer deposition on polymer based flexible packaging materials: Growth characteristics and diffusion barrier properties. Julkaisussa: Thin Solid Films. 2011 ; Vuosikerta 519, Nro 10. Sivut 3146-3154.

Bibtex - Lataa

@article{e7c8513e535b4dfdae5a1f28ae3589f1,
title = "Atomic layer deposition on polymer based flexible packaging materials: Growth characteristics and diffusion barrier properties",
author = "K{\"a}{\"a}ri{\"a}inen, {Tommi O.} and Philipp Maydannik and Cameron, {David C.} and Kimmo Lahtinen and Petri Johansson and Jurkka Kuusipalo",
note = "Contribution: organisation=epr pap,FACT1=1<br/>Publisher name: Elsevier",
year = "2011",
doi = "10.1016/j.tsf.2010.12.171",
language = "English",
volume = "519",
pages = "3146--3154",
journal = "Thin Solid Films",
issn = "0040-6090",
publisher = "Elsevier",
number = "10",

}

RIS (suitable for import to EndNote) - Lataa

TY - JOUR

T1 - Atomic layer deposition on polymer based flexible packaging materials: Growth characteristics and diffusion barrier properties

AU - Kääriäinen, Tommi O.

AU - Maydannik, Philipp

AU - Cameron, David C.

AU - Lahtinen, Kimmo

AU - Johansson, Petri

AU - Kuusipalo, Jurkka

N1 - Contribution: organisation=epr pap,FACT1=1<br/>Publisher name: Elsevier

PY - 2011

Y1 - 2011

U2 - 10.1016/j.tsf.2010.12.171

DO - 10.1016/j.tsf.2010.12.171

M3 - Article

VL - 519

SP - 3146

EP - 3154

JO - Thin Solid Films

JF - Thin Solid Films

SN - 0040-6090

IS - 10

ER -