Effect of pre-treatments on barrier properties of layers applied by atomic layer deposition onto polymer-coated substrates

Tutkimustuotosvertaisarvioitu

Standard

Effect of pre-treatments on barrier properties of layers applied by atomic layer deposition onto polymer-coated substrates. / Vähä-Nissi, M.; Hirvikorpi, T.; Sievänen, J.; Salo, E.; Harlin, A.; Johansson, P.; Kuusipalo, J.

13th European PLACE Conference 2011. Vuosikerta 1 2011. s. 447.

Tutkimustuotosvertaisarvioitu

Harvard

Vähä-Nissi, M, Hirvikorpi, T, Sievänen, J, Salo, E, Harlin, A, Johansson, P & Kuusipalo, J 2011, Effect of pre-treatments on barrier properties of layers applied by atomic layer deposition onto polymer-coated substrates. julkaisussa 13th European PLACE Conference 2011. Vuosikerta. 1, Sivut 447, Bregenz, Itävalta, 30/05/11.

APA

Vähä-Nissi, M., Hirvikorpi, T., Sievänen, J., Salo, E., Harlin, A., Johansson, P., & Kuusipalo, J. (2011). Effect of pre-treatments on barrier properties of layers applied by atomic layer deposition onto polymer-coated substrates. teoksessa 13th European PLACE Conference 2011 (Vuosikerta 1, Sivut 447)

Vancouver

Vähä-Nissi M, Hirvikorpi T, Sievänen J, Salo E, Harlin A, Johansson P et al. Effect of pre-treatments on barrier properties of layers applied by atomic layer deposition onto polymer-coated substrates. julkaisussa 13th European PLACE Conference 2011. Vuosikerta 1. 2011. s. 447

Author

Vähä-Nissi, M. ; Hirvikorpi, T. ; Sievänen, J. ; Salo, E. ; Harlin, A. ; Johansson, P. ; Kuusipalo, J. / Effect of pre-treatments on barrier properties of layers applied by atomic layer deposition onto polymer-coated substrates. 13th European PLACE Conference 2011. Vuosikerta 1 2011. Sivut 447

Bibtex - Lataa

@inproceedings{65029eca53a346c990cbfe224885a9f2,
title = "Effect of pre-treatments on barrier properties of layers applied by atomic layer deposition onto polymer-coated substrates",
author = "M. V{\"a}h{\"a}-Nissi and T. Hirvikorpi and J. Siev{\"a}nen and E. Salo and A. Harlin and P. Johansson and J. Kuusipalo",
year = "2011",
language = "English",
isbn = "9781618394392",
volume = "1",
pages = "447",
booktitle = "13th European PLACE Conference 2011",

}

RIS (suitable for import to EndNote) - Lataa

TY - GEN

T1 - Effect of pre-treatments on barrier properties of layers applied by atomic layer deposition onto polymer-coated substrates

AU - Vähä-Nissi, M.

AU - Hirvikorpi, T.

AU - Sievänen, J.

AU - Salo, E.

AU - Harlin, A.

AU - Johansson, P.

AU - Kuusipalo, J.

PY - 2011

Y1 - 2011

UR - http://www.scopus.com/inward/record.url?scp=84859608155&partnerID=8YFLogxK

M3 - Conference contribution

SN - 9781618394392

VL - 1

SP - 447

BT - 13th European PLACE Conference 2011

ER -